VELOX PLUS antivegetiva per eliche e piedi

Posted By :
Comments : Off
Special antifouling paint for propellers, stern drives, shafts and other underwater metallic parts. It provides outstanding  adhesion and efficacy. Resistant to galvanic currents, that are the main responsible of film detachments. Do not apply...
Read More

IDRON antivegetiva all’acqua

Posted By :
Comments : Off
IDRON is a revolutionary water-based antifouling paint. IDRON is a hard, non-soluble antifouling paint with a unique combination of binders and active principles. IDRON creates an extremely smooth and sliding surface even if applied with a...
Read More

BARRIER sistema epossidico strutturale

Posted By :
Comments : Off
Special epoxy coating featuring strong adhesion, high permeability and long-term mechanical properties like resistance and flexibility. Ideal for osmosis treatment, anticorrosive coating for metals, painting of wooden boats, can be used as a...
Read More

GRANIGLIA ANTISKID

Posted By :
Comments : Off

RAVVIVANTE PER TEAK

Posted By :
Comments : Off

[DILUENTE N. 4

Posted By :
Comments : Off

STUCCO EPOSSIDICO

Posted By :
Comments : Off

SVERNICIATORE FORTE

Posted By :
Comments : Off

MICROSFERE DI VETRO

Posted By :
Comments : Off

MICROFIBRE DI VETRO

Posted By :
Comments : Off

TAURUS

Posted By :
Comments : Off

Fiberglass

Posted By :
Comments : Off
SURFACE PREPARATION Degrease the surface with our antisilicone solvent SOLVENTE 102 and then sand it with medium sandpaper (n. 120-140). HULL – Apply one coat of FIBERGLASS PRIMER and wait at least 4 hours (at 20° C) – Apply one coat...
Read More

Steel or alluminium

Posted By :
Comments : Off
SURFACE PREPARATION Remove rust and scales from the surface through sandblasting. Remove dust using a dry cloth or an air jet (do not use any solvent otherwise adhesion of the following coat can be impaired). If necessary degrease the surface...
Read More

Wood varnishing

Posted By :
Comments : Off
After carefully sanding the wooden surface with medium sandpaper and dusting it, apply wet on wet 2-3 coats of our BARRIER TRASPARENTE diluted by 40-50% with our thinner DILUENTE N. 5, until the wood does not absorb anymore product. Let it dry...
Read More

Cast iron keels

Posted By :
Comments : Off
Remove rust and scales from the surface through sandblasting. Remove dust using a dry cloth or an air jet (do not use any solvent otherwise adhesion to the following coat can be impaired). If necessary degrease the surface with our antisilicone...
Read More

Osmosis

Posted By :
Comments : Off
OSMOSIS TREATMENT Sandblast the hull with coarse sandpaper, until the gel-coat is completely removed, if it is covered with blisters. In case a few  are present among the inner layers as well, these must be opened with a chisel one by one....
Read More

Propellers and stern-drives

Posted By :
Comments : Off
SURFACE PREPARATION Sand the surface with rather coarse and sharp sandpaper (n. 80 – 100) or sandblast it. Do not use worn out sand paper or metallic brushes, as they would polish the metallic surface rather than forming fine engravings,...
Read More

Wood

Posted By :
Comments : Off
SURFACE PREPARATION The first step in the painting cycle of wooden boats is the priming of the wood with our epoxy protective coating BARRIER, which features great adhesion on wood and an excellent protective power. Sand the dry wooden surface...
Read More

ECO

Posted By :
Comments : Off

TRITON

Posted By :
Comments : Off

NEPTUNE

Posted By :
Comments : Off
Scroll Up